Heat slowly and uniformly to 1,450 deg.F. and forge thoroughly. Do not under any circumstances attempt to harden at the forging heat. After cooling from forging reheat to about 1,450 deg.F. and cool slowly so as to remove forging strains. ... Read more of Oil-hardening Steel at Steel Making.caInformational Site Network Informational